Inconel 718 is a high-strength, high-temperature, corrosion-resistant nickel-based alloy whose chemical composition covers nickel, chromium, molybdenum, iron, cobalt, aluminum, titanium, zirconium, carbon, and manganese. Inconel 718 has a melting point of 1430°C and displays effective heat and temperature resistance. This nickel superalloy can create a strong and stable oxide layer when heated. In addition, the layer makes this Inconel variant significantly resistant to oxidation, thus protecting it from corrosion. Inconel 718 bar can be manufactured through a variety of processing methods, such as forging, hot rolling, cold drawing and welding. It is prone to oxidation and hardening at high temperatures, and appropriate preheating and post-processing measures are needed to prevent the phenomenon.
Product Name | Inconel 718 Bar | |
Outer Diameter | Round Bar | 4mm-500mm |
Hexagon Bar | 18mm-57mm (11/16″ to 2-3/4″) | |
Square Bar | 18mm-47mm (11/16″ to 1-3/4″) | |
Flat Steel | 1/2 "to 10", Thickness: 2mm-150mm, Can provide customized | |
Length | 1-6 meters, Length can be customized | |
Standard | ASTM, AISI, JIS, GB, DIN, EN, etc. | |
Surface | Black, Bright Polished, Rough Turning, Matt Surface Treatment, NO.4, BA, etc. | |
Certificate | ISO, SGS, BV | |
Production Technology | Hot Rolling, Cold Rolling | |
B | C | Al | Si | P | S | Ti | Cr | Mn | Fe | Co | Ni | Cu | Mo | Cb (Nb Ta) |
0.006 max | 0.08 max | 0.20-0.80 | 0.35 max | 0.015 max | 0.015 max | 0.65-1.15 | 17.00-21.00 | 0.35 max | Remainder | 1.0 max | 50.00 - 55.00 | 0.30 max | 2.80 - 3.30 | 4.75 - 5.50 |
Tensile Strength (ksi) | 0.2% Yield Strength (ksi) | Elongation% in 2 inches |
180 | 150 | 12 |
Units | Temperature in°C | |
Density | 8.19 g/cm³ | Room |
Specific Heat | 0.104 Kcal/kg.C | 21° |
Melting Range | 1260-1366°C | - |
Modulus of Elasticity | 199.9 KN/mm² | 21° |
Electrical Resistivity | 125 µΩ.cm | Room |
Coefficient of Expansion | 13.0 µm/m °C | 20 - 100° |
Thermal Conductivity | 11.1 w/m-° K | 21° |
This nickel steel alloy can be manufactured rapidly and can be welded in an annealed or precipitation (age) hardened condition. This superalloy is used as part of various commercial enterprises, such as aerospace, marine engineering, chemical processing, pollution control equipment and nuclear reactors.